Hunan Deson New Material Co., Ltd
+8613873121965
Method For Making Colored Asphalt Pavement With Asphalt Pigment - Application Guide

Method For Making Colored Asphalt Pavement With Asphalt Pigment - Application Guide

Step‑by‑step guide for producing colored asphalt pavement using iron‑oxide asphalt pigment. Covers crushed stone, pigment dosage, decolorized asphalt oil ratio, mixing temperature 130‑150℃, and spreading & compaction process for landscape road and playground.
MOQ:1 ton | Free sample available | TDS & MSDS on request

Send Inquiry
  • Description

    Introduction

    Colored asphalt pavement brings aesthetic, traffic‑safety and environmental value to landscape roads, park paths, running tracks, bike lanes and pedestrian areas. Compared with conventional black bitumen pavement, colored asphalt creates attractive color zones, improves visual guidance for vehicles and pedestrians, and reduces heat absorption on sunny days.

    The production process is similar to traditional black bitumen, but uses three key raw materials: crushed stone aggregate, asphalt pigment powder and decolorized asphalt oil. Below is the recommended mixing procedure and dosage reference.

     

    Raw Materials

    1, Crushed Stone Aggregate - Clean, dry crushed stone with even particle size as the main skeleton of the mixture.

    01

    2, Asphalt Pigment Powder - High‑temperature‑resistant iron‑oxide inorganic pigment (red, yellow, blue, green, gray, orange available) that provides stable color under hot‑mixing condition.

    02

    3, Decolorized Asphalt Oil - Transparent / decolorized bitumen binder that replaces black bitumen to keep the pigment color visible.

    03

    Samples From The Lab

    04

    The difference between colored asphalt and black bitumen

    The process and the facility is very similar with the black bitumen.

    product-1-1

    product-1-1

    product-1-1

    A:The difference is about the temperature, different color, the temperature will be different.

    B: At meanwhile we will use the colored pigment powder to replace the mineral powder.

    C: We will use the decolorized asphalt oil instead of the black bitumen.

     

    Recommended Mixing Method

    1. Preheat the crushed stone to target temperature 130‑150℃ (e.g. 130‑150℃ for blue asphalt).
    2. Add asphalt pigment powder at recommended dosage (about 3% by weight of stone) together with decolorized asphalt oil (about 5% by weight of stone) in proportion.
    3. Stir evenly and keep the temperature within 130‑150℃ during the whole mixing process to ensure uniform pigment dispersion.
    4. Discharge the mixed material, then spread and compact immediately to obtain the finished colored asphalt pavement.

     

    Recommended Pigment Dosage Reference

    Pigment Name

    Area
    (㎡)

    Thickness
    (cm)

    Crushed Stone Density
    (t/m³)

    Crushed Stone Weight
    (Ton)

    Material Addition ratio

    Material Weight
    (Ton)

    Temperature Range
    (℃)

    Asphalt Pigment Red

    1000

    5

    2.35

    117.5

    2.50%

    2.94

    140-170

    Asphalt Pigment Yellow

    1000

    5

    2.35

    117.5

    3.00%

    3.53

    130-150

    Asphalt Pigment Green

    1000

    5

    2.35

    117.5

    3.00%

    3.53

    130-150

    Asphalt Pigment Blue

    1000

    5

    2.35

    117.5

    3.00%

    3.53

    130-150

    Asphalt Pigment Gray

    1000

    5

    2.35

    117.5

    2.50%

    2.94

    130-150

    Asphalt Pigment Orange

    1000

    5

    2.35

    117.5

    2.50%

    2.94

    130-150

    Discolored Asphalt

    1000

    5

    2.35

    117.5

    5.00%

    5.88

    130-150

    Note: The original page listed per‑1000kg amounts. We re‑organized them into clear columns. Dosage may be adjusted according to target color depth and local aggregate condition.

     

    Key Benefits & Quality Tips

    ‑ Stable color under hot‑mixing: use high‑temperature‑resistant iron‑oxide asphalt pigment to avoid fading during 130‑150℃ mixing.

    ‑ Keep mixing temperature under control (130‑150℃); avoid over‑heating which may cause color shift or binder degradation.

    ‑ Ensure uniform dry‑mixing of pigment with aggregate before adding oil, to prevent color spots.

    ‑ Compaction should be completed while the mixture is still warm for a smooth, even surface.

    ‑ Iron‑oxide pigments offer good weather & UV resistance for long‑term outdoor pavement color retention.

     

    Asphalt Pigment Series Available

    Red | Yellow | Blue | Green | Gray | Orange - Please contact us for detailed TDS and recommended grade for your colored‑asphalt project.
    Discharging after Stir and Heat (Red)

    11

    Spread (Red)

    12

    Compacted (Red)

    13

    Discharging after Stir and Heat (Blue)

    14

    Spread (Blue)

    15

    Compacted (Blue)

    16

    Packaging & Loading

    ‑ 25kg woven bag lined with inner plastic bag, palletized

    ‑ 20GP container loading: about 24‑25 tons

     

    Inquiry Now

    Send your inquiry today to lucy@desonpigment.com or WhatsApp +86 138 7312 1965.

    Tell us your target color and project type, we will recommend suitable asphalt pigment grade and provide TDS, MSDS and free sample.

    We will reply you within 12 hours.

    Hot Tags: Method For Making Colored Asphalt Pavement With Asphalt Pigment - Application Guide, China Method For Making Colored Asphalt Pavement With Asphalt Pigment - Application Guide suppliers, manufacturers, factory, Color Asphalt Pigment, Iron Oxide For Asphalt, Asphalt Pigment, Asphalt Colour Paint, Iron Oxide Grey, Bitumen Pigment